It is installed in Oil Refinery…..

 

Regards,

Vinod Kataria

 

 

From: materials-welding@googlegroups.com <materials-welding@googlegroups.com> On Behalf Of gulzar ali
Sent: 28 May 2020 13:34
To: materials-welding@googlegroups.com
Subject: Re: [MW:30922] SS-316L Rusting

 

 

What type fluid service? 

 

 

 

On Thu, May 28, 2020, 10:22 AM 'Karthik' via Materials & Welding <materials-welding@googlegroups.com> wrote:

It might be due to poor cleaning/pickling process or no pickling and or improper picking/curing time

Thanks& Regards,

 

(Karthik)

Karthikeyan.S

M: +66-892512282
E-mail : karthik6684@yahoo.com


On Thursday, May 28, 2020, 12:16:41 PM GMT+7, Vinod Kataria <vinod.kataria@blissanand.com> wrote:

 

 

Dear Expert,

We have received an email from our customer with pictures showing "rust" on the stainless steel (SS-316L) chambers.  Can anyone please tell me what you see in these pictures from your perspective?

 

 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/TY2PR0101MB29421148FFC32992DCB565C5878E0%40TY2PR0101MB2942.apcprd01.prod.exchangelabs.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/11782024.592550.1590643196107%40mail.yahoo.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAH%2BZiM_GBiUFEfyz1w5RtE4LMSxmHPr0QoabbNOnH3Fv_iXMKQ%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...