Re: [MW:30910] AWS D1.1 -Combination of welding process

I don't think there is any provision to derive a WPS for a single process from a multi process PQR in AWS D1.1. kindly check.

On Sat, 23 May 2020, 08:47 'Rajnish Dixit' via Materials & Welding, <materials-welding@googlegroups.com> wrote:
Dear Chintan,
Yes, you can use this WPS for any one welding process also within the qualification ranges of that particular process.

Thanks,
Regards,
Rajnish Dixit
On Wednesday, 20 May, 2020, 10:32:35 pm GMT+7, Chintan Raval <chintan51@gmail.com> wrote:


Dear all 
Kindly advice 
I have WPS for weld process fcaw + saw as per aws d1.1 

I want to use same wps for only FCAW process as saw is not feasible for few joints.

Is this allowed as per aws d1.1 or new pqr is required for single process.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOdsS43qnrwOjNUDrkcjGozo42GT7AMERLLxmpvPieJ6ZbH0yw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1485215300.2498535.1590207623827%40mail.yahoo.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFS9gDOrA8gZ2WjT2tCQC0NtY3Fh11s6rcvDfrc9qkWQ-3Lp6w%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...