what is design and operating temperature of 347 ? is it pressure application ?
Stabilizing treatment needs some in application if there is risk of  SRC 
similarly please let me know what is the application of 310 
On Fri, May 22, 2020 at 9:53 AM Arun Nair <arunnair.mundakkal@gmail.com> wrote:
Hello,--Weld joint between SS310 to SS347 kindly advice about heat treatment require or not? Either pre or post.ArunNair
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAM8%3Dvxqa%2BZJyP4_idWdODyDJCK27L2VO1EPvGdgqtbN%2Bikxqdw%40mail.gmail.com.
--
Regards
Kural
        -- Kural
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CABhoKTBgQvuxUdU%2B-5byBwCL5Q2pcsZVw701KMvxqBix%2Bem2cQ%40mail.gmail.com.
Comments