seat test and closure test  - Same.

Back seat test - The Gate / Globe valve in full open condition.
The  Stem ( Back seat ) lock the stem bush in the bonnet to avoid leakage.

Shell test - Partial open -  1.5 times design pr 
Back Seat - Full Open    - 1.1 times design pr  
Seat Test - Full close  -     1.1 times design pr 

Best Regards
Kingsly Geo


On Wed, 8 Apr 2020 at 08:20, <rawat.sing@gmail.com> wrote:
What is difference between seat test and closure test.
What is the required position of gate during back seat test.
Regards

Rawat

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/bb49cbfd-44ef-411d-b710-d45b3d0cb951%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAAR7VZ_s8BrsCdo4HeYTZgjyDqb%3Dg5VB2M_r78f9BHPQr32J7w%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...