Use 9018-G 

On Sun, 17 May 2020 1:37 pm Khul ke jiyoo kya pata Kaal hoo na hooooooo, <bapunchandra@gmail.com> wrote:
Thanks for the response.
My straight requirement is as follows
Pipe-API 5L x 70 Thickness 17 mm
Welding requirement-Automatic orbital welding
Use-Cross country pipeline
Kindly provide Best suitable welding consumables Or can share any specific PQR
Thanks
Cam


Sent from my iPhone

> On 17-May-2020, at 11:37 AM, Chintan <chintan51@gmail.com> wrote:
>
> Use E7018 if pwht not required
> Use E8018 G if pwht & impact required
>
> --
> https://materials-welding.blogspot.com/
> https://www.linkedin.com/groups/122787
> ---
> You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
> To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
> To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/ed350fee-d313-4c37-894a-ca3280cf1d8c%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/E207FACD-89C3-421B-A8E8-8BF006259BE0%40gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eO8Y_EYCV3-F7vexVR23FUSnqp0jTW6rf_uU%3Do%3DzkfJ1Q%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...