Re: [MW:30875] Welding of DissimilThickness

It is normal practice, we weld flanges to cylinder tubes with even more thickness difference. You just need to modify the weld joint accordingly.

Regards
Chris

On Thu, May 14, 2020 at 15:43 george keribo <berepele@gmail.com> wrote:
Team i want to know how it can be possible to weld materials with dissimilar wall thickness of 5mm. DSS pipes to flanges. Flanges are higher than the pipes in thickness with 5mm.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/7260e93e-ba08-4cad-897e-69efa75f095c%40googlegroups.com.
--
THANKS AND REGARDS
CHRIS SABU
0559695451

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CACY3QXRciy7ETQTUN8SazWz_DqoUy7jWNuM7GnkDkAS2dfBYLw%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...