If ID is same then weld both pipe to flange and provide taper transition on flange of minimum 15mm.

Regards,

Zakir Ali.

Sent from RediffmailNG on Android




From: george keribo <berepele@gmail.com>
Sent: Thu, 14 May 2020 17:13:57 GMT+0530
To: Materials & Welding <materials-welding@googlegroups.com>
Subject: [MW:30874] Welding of DissimilThickness

Team i want to know how it can be possible to weld materials with dissimilar wall thickness of 5mm. DSS pipes to flanges. Flanges are higher than the pipes in thickness with 5mm.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https:roups.google.com/d/msgid/materials-welding/7260e93e-ba08-4cad-897e-69efa75f095c@googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1589456637.S.7589.16779.f5-224-105.1589477753.5913%40webmail.rediffmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...