Your leg length is 5 mm or less. Penetration may be reached 5 mm or less so take 26 mm. 

Regards, S.SENTHILKUMAR


On Wednesday, 13 May, 2020, 04:31:41 pm IST, Ilkin Hasanov <ilkinhasanov.91@gmail.com> wrote:


Hi Gents,
We have a partial penetration (S=21mm)  with  5 mm leg length joint configuration ; (Tee Joint - combination weld (partial pen + fillet weld)
As per Client requirements if reference thickness is more than 25mm NDT should performed after 48 hours. (Reference thickness is

Could you please advise in our case what is the reference thickess 21 or 26 mm (21mm+5mm)



Regards,
Ilkin Hasanov.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADrxeDYx_%3DoAOWk_S4Swb7CzdC9zWF%3DTEHEbhorJzb8QiZG6Hg%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...