Monday, May 11, 2020

Re: [MW:30862] PWHT Requirements and Material Selection

Refer Table 1 for NACE SP0472  for PWHT requirement and its exemption.

Thanks
Atul Khatri

On Sun, May 10, 2020 at 9:01 AM George Dilintas <dilintas@gmail.com> wrote:
In sour service there is a HIC risk. This risk is reduced if PWHT is done even the weld thickness is lower than the limits of UCS-56-1

Στις Τρί, 5 Μαΐ 2020, 07:28 ο χρήστης enginakgun55 <enginakgun55@gmail.com> έγραψε:
Hello,

We work on material selection about column materials (shell, head, skirt). If we use A-516 Gr.70 material in this project, does it require heat treatment for repair on the column during maintenance?


Production Properties : Sour Service , Distilation Column

Best Regards

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/c8e5362b-3f5e-4fdc-912f-cc390d512800%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40CKPaDH-qJdi%3DN9_Ra6wRcBgo%3DpDhg4qSFt77uGX2iBXQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CACKOSeCRObn4YCM6QP%3Dka8uBi9ubKsByRQWSLKrBFpY_hXB_Tw%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...