RE: [MW:30851] ISO 9606 vs EN 287-1

There are only small formal differences. EN 287-1, was a pure European norm and has been withdrawn, because it was changed to an international standard (ISO).

Further EN 287.1 was harmonized to the old Pressure Equipment Directive (PED), 97/23/EC where ISO 9606-1 is harmonized to the new PED, 2014/68/EU.

 

Kind regards

Kristian Lund Jepsen

Lead Specialist, Piping, Mechanical & Layout

 

D +45 23402936

M +45 23402936

kuj@ramboll.com

Rambøll Danmark A/S, DK REG. NO. 35128417
Registered office: Hannemanns Allé 53, 2300 Copenhagen S

 

From: materials-welding@googlegroups.com <materials-welding@googlegroups.com> On Behalf Of Ilkin Hasanov
Sent: 7. maj 2020 14:05
To: materials-welding@googlegroups.com
Subject: [MW:30850] ISO 9606 vs EN 287-1

 

Gents,

 

Could you please help me to clarify for myself difference of  ISO 9606 vs EN 287-1???

 

 

BR,

Ilkin Hasanov 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADrxeDbG5zAG%3DaAXDoiSK5eo%3DXHXFzQi8y4pjyeK4bg9C7uUHA%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...