Re: [MW:30846] PWHT Requirements and Material Selection

The material 516 Gr 70 is a P1, you are mentioning that it is a repair, I suggest you check Table UCS-56-1 (b) (ASME Section VIII Div. 1), where the PWHT requirements for P1 materials appear, in ( b) it makes some exceptions to the PWHT based on the thickness of the material, if you exceed those thicknesses you will have to do the PWHT, but because it is a repair you also have to check the NB-23 and API 650 since from what I see in the drawing is a kit for the O&G Industry.
The Skirt I do not think it should carry PWHT since it is not a pressurized part.
Cheers!.

El mar., 5 may. 2020 a las 1:31, 'TC Kwa' via Materials & Welding (<materials-welding@googlegroups.com>) escribió:
Hi,

If it is for Sour service, PWHT shall be done, since material is A-516 Gr 70.
Thank you. 


Regards,

Ir. TC Kwa

+6012-3998739

Email: tckwa@yahoo.co.uk

LinkedIn Profile : https://my.linkedin.com/in/tckwa 





On Tuesday, 5 May 2020, 12:36:46 GMT+8, enginakgun55 <enginakgun55@gmail.com> wrote:


Hello,

We work on material selection about column materials (shell, head, skirt). If we use A-516 Gr.70 material in this project, does it require heat treatment for repair on the column during maintenance?


Production Properties : Sour Service , Distilation Column

Best Regards

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/c8e5362b-3f5e-4fdc-912f-cc390d512800%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/601900513.2557215.1588657191572%40mail.yahoo.com.


--

Ing. José Juan Jiménez Alejandro

Independent Consultant in Parts

and Pressure Equipment

SSI-TPI

Móvil +52 1 812 352 4606

Skype: jjjimeneza





--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAO5ZurJzZKoh7ksS5u6LqF5ozWO2rKeVaW0rOOMLTtepqCWsaA%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...