Tuesday, March 19, 2019

Re: [MW:29313] What is Deference Between LP & HP welder?

Dear Sir,


HP & LP welders are a general classification of pipe welders regardless of construction code.
In combined cycle power plant projects in Bangkok and Myngyan (Myanmar) We 've Catagorised 6G Carbon steel pipe welders as LP and 6G low alloy Pipe welders as HP.

HP welders used to weld P11,P22,P91 pipes connecting boiler which require pre&post weld heat treatment . Mean time LP welders engaged in CS pipes carrying cooling water .
Above catagarisation used for fixing their wages also. HP will get more bucks than LP.

Since both are qualifying in 6G position, there is no question of position variation like 1G,4G etc.
1G,2G, 3G, 4G are plate welding , economicaly for this another group -structural welders - can be used if available. 

Regards,

JIJILAL K M,
Lead QA/QC
Corrtech Intl. Ltd.
BPCL HTPL Project,
Kochi Refinery. South India.




On Thu, Mar 7, 2019, 22:00 Atif <atif.aslam@bishoinfra.com> wrote:
Dear Sir,

Regarding HP piping qualified welder can perform LP piping job?
and LP piping qualified welder can perform also HP piping job let me know pls.

Another question is that there is any variation of test Position e.g. 1G, 2G, 3G, 4G etc. for the welder test between HP & LP ?

regards:
Atif.  

On Thursday, March 7, 2019 at 9:43:50 AM UTC+6, etan wrote:
Dear Atif,
HP Means, High-Pressure pipes and pipe materials alloy or low alloy steel
LP means, Low-Pressure pipes materials carbon steel. So you have to know pipe materials and according to materials you need to qualify welders.

Regards,

Eyup Tan



On Wed, Mar 6, 2019 at 10:15 AM Atif <atif....@bishoinfra.com> wrote:
Dear All,
Our client is asking for make categories for our welder such as HP & LP,  in Combined cycle power plant project, anybody can help me that why we need to do this and what is the welder qualification testing procedure/system for HP & LP welder? 

Regards:
Atif.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...