Tuesday, March 19, 2019

Re: [MW:29313] Build up material Non-Magnetic Stabilizer P550

Dear Mr. Bien

try this electrode 

EFeMnCr

Best Regards ,
ENG. Ahmed Othman
+966 534311070


On Monday, March 18, 2019, 6:54:53 p.m. GMT+3, weldinginspections.net <bck055@gmail.com> wrote:


Hi All,

Could you advise type/brand name of welding consumables which use to build up for Non-Magnetic Stabilizer P550.
Material properties link: https://www.sbsaleshouston.com/P550.html


Thanks
Bien ND

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...