Re: [MW:29310] RT Sensitivity Not Achieving for Pipe 1 1/2 " Sch 40

Dear sir,

Thanks for your immediate response

We have tried using D4 Film & Increased SFD also,
but still the issue remains the same.

Regards
Vikram Saipogu

On Tue, Mar 19, 2019, 11:17 AM Paresh Patel <pkpatel1968@gmail.com> wrote:
Try for fine grain/ slow film, use low Curie source.

On Mon 18 Mar, 2019, 9:24 PM vikram saipogu, <saipoguvikram@gmail.com> wrote:
Dear All,

Please provide me some suggestion,

How shall I achieve sensitivity for lower thickness and lower diameter pipe using Gamma Rays i.e Iridium 192 ?

Client requirements is Radiography by Gamma Rays 

Thanking you


Best Regards,

Vikram Saipogu


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...