Monday, March 18, 2019

Re: [MW:29293] Hydro test pressure gauage range

Yes as per asme sec viii div 1 you can you pr gauge with in the range of 1.5x - 4x of the pressure required.

-- 


Thanks & Regards,

Sunny Modi
Mobile:- +91-8130365765

On Sun, Mar 17, 2019 at 2:45 PM Mithlesh <mithleshmech47@gmail.com> wrote:
Hii

My hydro pressure required is 61kg/cm2 and i used dial range 0-120kg/cm2 is it acceptable as per IBR?.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...