Friday, March 15, 2019

Re: [MW:29272] As per AWS D1.1-2015

That's one hell of a TPI...


Ramin  Kondori
Sr. QA/QC & Welding Engineer
-----------------------------------------------------------
PG-Dip. in Welding Engineering (IWE  AT  0070)
BSc. in Civil Engineering (IUT)
BGAS Painting Inspector
ASNT Level I&II
                        
IIW-Logo-Colour-small


On Fri, Mar 15, 2019 at 6:31 PM Kiran <karan.hbl@gmail.com> wrote:
Dear Experts,

Please need your help regarding my queries as below as per AWS D1.1-2015.

1) SMAW process is only applied to Material S275JR .

2) S355JR & Gr I&II Fit up tack will be done by GMAE or FCAW.

3) Gr I&II to S355JR welding not allowed.

4) As per D1.1 welding in OH postion is not allowed.

5) Gr I&II only GMAW is allowed.

6) S275JR, S355 JR welding FCAW is allowed.

above all comments received from our TPI Inspector can you please explain with clause as per AWS D1.1.

Thanks and Regards
Kiran   

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35354] Cast-iron welding

1. Preheat joint area(other area, cover with mineral wool). 2. ENiCi or ENiFe-CI. 3. stringer bead. 4. peening is to be done on weldmetal im...