Hi folks,

Correct me if I am wrong. If the code of construction is B31. 3, LP refers to Low pressure piping  which is Chapter V design and requirements while HP refers to High pressure piping Chapter IX design and requirements. Chapter IX is very stringent in its material selection,welding procedure qualification, welders qualification and NDE acceptance.  Change in material grade, heat treatment condition is essential. Impact toughness is mandatory for WPQT, PWHT is mandatory for butt welds, welder qualification requires impact toughness testing. The thickness are project specific as it  pressure temp rating is greater than  2500#. There are more to it. 

On Wed, Mar 6, 2019, 11:15 AM Atif <atif.aslam@bishoinfra.com> wrote:
Dear All,
Our client is asking for make categories for our welder such as HP & LP,  in Combined cycle power plant project, anybody can help me that why we need to do this and what is the welder qualification testing procedure/system for HP & LP welder? 

Regards:
Atif.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35614] Re: SS FILLER

dear , pl check A number and Gas composition use for ss cant be sutibale same % for duplex., u need to qualified with aditional testing of f...