Re: [MW:29242] Hot Tap welding Procedure -Welding Code

Follow B-31.3 as per design code

On Sat, Mar 9, 2019 at 10:37 AM Sureshkumar Pethureddy <sureshrnr@gmail.com> wrote:
Dear sandeep

The execution of "hot-tap" branch connections onto piping systems and pipelines containing hydrocarbons under operating conditions. It has been developed to reflect current understanding of the technology and to improve safe practices in the field. It is intended to cover hot-tapping on carbon, carbon-manganese and high-strength low-alloy steels.

Due to the distinction made in the relevant standards between on-plot piping and off-plot pipelines or flow lines, a similar distinction is sometimes made within but this has been avoided wherever possible. Additionally, it is assumed that the piping systems are designed and operated in accordance with ASME B31.3 and pipeline systems are designed and operated in accordance with ISO 13623, ASME B31.4, or ASME B31.8, or a combination.

.WPS Welding procedure specification

NOTE: Some parts of a pipeline system, although physically located "off-plot", may be designed in accordance with ASME B31.3. For the  purposes of piping shall be considered to be on-plot. Similarly, some refinery piping, although physically located "on-plot", may be designed in accordance with ISO 13623, ASME B31.4 or B31.8. such piping shall be considered to be off-plot.

Regards

suresh



On Fri, Mar 8, 2019 at 11:40 AM sandeep k sreedhar <sandeepkelakam@gmail.com> wrote:
Dear Experts
Greetings!
I have hot tap welding in my scope of work, According to  P&ID the hot tap is coming under the design code B31.3. 
The Hot tap welding requirement are as follows as per the client specification- ADNOC Group.

The CONTRACTOR/VENDOR shall follow procedures and qualifications specified in DGS 6300-001- WELDING AND NDE OF PIPING SYSTEM (Based on Section IX) for On-Plot Piping and DGS 6300-004- Welding and NDE of pipeline  for Off-Plot Piping- .
Welders shall be qualified in accordance with DGS 6300-001 for On-Plot Piping and DGS 6300-004 for Off-Plot Piping. 
For Off-plot pipelines, both the procedure and the welders should be qualified using a full-scale simulation of the connection, in accordance with API 1104 or equivalent COMPANY‟S specification. 

All the Hot tap sub contractor's proposing API 1104 based WPS since considering the service welding requirement.

Now I am confused which welding code has to be followed. Request for yours  kind advise on the same.


Regards

SANDEEP K SREEDHAR

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35354] Cast-iron welding

1. Preheat joint area(other area, cover with mineral wool). 2. ENiCi or ENiFe-CI. 3. stringer bead. 4. peening is to be done on weldmetal im...