Dear Sir,
On Thursday, March 7, 2019 at 9:43:50 AM UTC+6, etan wrote:
-- Regarding HP piping qualified welder can perform LP piping job?
and LP piping qualified welder can perform also HP piping job let me know pls.
Another question is that there is any variation of test Position e.g. 1G, 2G, 3G, 4G etc. for the welder test between HP & LP ?
regards:
Atif.
On Thursday, March 7, 2019 at 9:43:50 AM UTC+6, etan wrote:
Dear Atif,HP Means, High-Pressure pipes and pipe materials alloy or low alloy steelLP means, Low-Pressure pipes materials carbon steel. So you have to know pipe materials and according to materials you need to qualify welders.Regards,Eyup TanOn Wed, Mar 6, 2019 at 10:15 AM Atif <atif....@bishoinfra.com> wrote:Dear All,--Our client is asking for make categories for our welder such as HP & LP, in Combined cycle power plant project, anybody can help me that why we need to do this and what is the welder qualification testing procedure/system for HP & LP welder?Regards:Atif.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com .
Visit this group at https://groups.google.com/group/materials-welding .
For more options, visit https://groups.google.com/d/optout .
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.
No comments:
Post a Comment