Re: [MW:29183] How to qualify WPS ?

QW-211 BASE METAL
The base metals may consist of either plate, pipe, or
other product forms. Qualification in plate also qualifies
for pipe welding and vice versa. The dimensions of the test
coupon shall be sufficient to provide the required test
specimens.

Groove-weld test qualifies for fillet welds for all thickness and diameters.

On Tuesday, February 12, 2019 at 8:15:56 PM UTC-6, Souravbohray wrote:
sir i want to make it easy to those people who are fresher i know just make a wps of 6g position it will be done for all except what welding process we used

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35354] Cast-iron welding

1. Preheat joint area(other area, cover with mineral wool). 2. ENiCi or ENiFe-CI. 3. stringer bead. 4. peening is to be done on weldmetal im...