As per API598
Closure test:pressure test used to confirm leakage past or through a valve closure mechanism.
The closure test pressure obtained as follow:
-low pressure closure test 4-7 barg
-high pressure closure test=110% maximum allowable pressure
As you can see the closure test pressure is different from shall test pressure which is 150%MAWP.
Also, do a search forn FCI-20

On Thursday, January 31, 2019 at 4:45:48 AM UTC-6, chiluka venkatramulu wrote:
Dear All,,
Is the Valve closer test means sheet leak test or body pneumatic test?

Venkatramulu

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35354] Cast-iron welding

1. Preheat joint area(other area, cover with mineral wool). 2. ENiCi or ENiFe-CI. 3. stringer bead. 4. peening is to be done on weldmetal im...