[MW:29259] Electrode selection for 3G40 to ST52-3


hello dear expert
? Do you know what kind of electrode is suitable for welding 3G40 to ST52-3

Thanks

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35614] Re: SS FILLER