Thursday, March 7, 2019

[MW:29211] WELDING CONSUMABLE SELECTION FOR DISSIMILAR MATERIAL

Dear All,

I have to weld SA 213 TP 304 tubes to SS 410 (plate) cladded on SA 266 cl 2 (forged tube sheet).

Which Filler Wire has to be used.

As per my calculation, I am going with 309 Mo, Is it OK ?

Please reply, its urgent.

Thanks and Regards

Sunny Modi
8130365765
Manager QA/QC
M/s MAPL

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35738] ASME IX WPS Qualification Query: GTAW + FCAW with Multiple PQRs

Dear Welding Experts, I'm currently preparing a Welding Procedure Specification (WPS) and have encountered a request to qualify a GTAW +...