There is nothing HP & L.P welder as per code.
On 7 Mar 2019 9:13 am, "Eyup Tan" <eyuptan@gmail.com> wrote:
Dear Atif,HP Means, High-Pressure pipes and pipe materials alloy or low alloy steelLP means, Low-Pressure pipes materials carbon steel. So you have to know pipe materials and according to materials you need to qualify welders.Regards,Eyup Tan--On Wed, Mar 6, 2019 at 10:15 AM Atif <atif.aslam@bishoinfra.com> wrote:Dear All,--Our client is asking for make categories for our welder such as HP & LP, in Combined cycle power plant project, anybody can help me that why we need to do this and what is the welder qualification testing procedure/system for HP & LP welder?Regards:Atif.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com .
Visit this group at https://groups.google.com/group/materials-welding .
For more options, visit https://groups.google.com/d/optout .
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com .
Visit this group at https://groups.google.com/group/materials-welding .
For more options, visit https://groups.google.com/d/optout .
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.