Monday, July 23, 2018

Re: Re: [MW:28107] FABRICATION TRAVELLAR FORMATE (FOR HEAT EXCHANGER OR PRESSURE VESSEL)

ITP is being prepared based on process proposed sequence. In Traveller, production people is also taking responsibility by signature

On Mon, 23 Jul 2018 8:12 am Nithin Joseph, <nithindsilva4u@gmail.com> wrote:
Hi traveller is nothing but ITP. So no point in maintaining 2 documents.

On Sun, Jul 22, 2018 at 8:46 AM, Jay Poojary <jayogini@gmail.com> wrote:
Mr Jay Prajapati, 

This are not code requirements, this seems to be specific client requirements. Similar of this type we have for our orpic projects which is called Readiness program. 



On Sun, Jul 22, 2018, 8:37 AM jay prajapati <jay0000.jp@gmail.com> wrote:
Thanks dear,

Reference to trailing mail,
But i have also one formate which is different from ITP. which is given in detailed,(find attached file)

Now my question is.
Is ITP and traveler both are same things or different? 
If there is any other formate like this( attachment) then please provide, so i can make traveler in details by examine one or more.

On Sat, Jul 21, 2018 at 10:10 AM 'Shashank Vagal' via Materials & Welding <materials-welding@googlegroups.com> wrote:
You can always make it from an ITP.

Best Regards,

Shashank C Vagal (Quality Adviser), (+91) 8082395502, 8779046302,

NEO METAL-ANALYST & NDT SERVICES

·       A-25, Geet Siddhi, Boradevadi, Moshi-Haveli, PCMC, Pune 412105

·      301, PRATHAMESH, M G Rd – Mahant Rd, Vile Parle East, Mumbai 400 057 INDIA

www.neometalanalystndt.com / enquiry@neometalanalystndt.com / nach_sam@yahoo.com




On Friday, 20 July, 2018, 5:49:58 PM IST, muneebslsa@gmail.com <muneebslsa@gmail.com> wrote:


FYI



____________ 

Thanks & Regards,

MOHAMED          MUNEEB           MAHABOOB

JAPID

JAZAN-IGCC-001

M:                         +966(0)59 607 2237

O.E:     mahaboob.muneed@aramco.com

P.E:                  muneebslsa@gmail.com

 
Date: 2018-07-19 14:44
Subject: Re: [MW:28095] FABRICATION TRAVELLAR FORMATE (FOR HEAT EXCHANGER OR PRESSURE VESSEL)
fyi pl (Traveller)

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349

On Thu, Jul 19, 2018 at 1:39 PM, JAY <jay0000.jp@gmail.com> wrote:
Dear professional, 


I just had my customer come see my shop and they asked me if I use 
shop travelers. I had to tell them no because I don't right now. I want to start using one but am having trouble finding a template online. Does anybody have a template, or a copy of one that I can use to make one?

Please Do the needful.

--
https://materials-welding. blogspot.com/
https://www.linkedin.com/ groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@ googlegroups.com.
Visit this group at https://groups.google.com/ group/materials-welding.
For more options, visit https://groups.google.com/d/ optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.



--
Regards,
Dsilva

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...