Thursday, July 26, 2018

Re: [MW:28136] Regarding 2% sensitivity in radiography film.

IQI always in source side subject to accessibility required, otherwise IQI will place on film side that time IQI size/nos will be as per code.   

Thanking you,


P.K.MAJI
Sr Surveyor,
BUREAU VERITAS (I) PVT LTD.,
e-mail:-prabir.maji@in.bureauveritas.com
NAGPUR,
www.bureauveritas.co.in
Mob:9422127912


From: Souravbohray <ermechsouravbohray@gmail.com>
Sent: Wed, 25 Jul 2018 11:10:38
To: Materials & Welding <materials-welding@googlegroups.com>
Subject: [MW:28134] Regarding 2% sensitivity in radiography film.

is IQI is source side or film side

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...