Thursday, July 19, 2018

Re: [MW:28095] USE OF ELECTRODE

you can use but not reverse if impact was done

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349

On Tue, Jul 17, 2018 at 8:39 PM, Hasin Shaikh <hasin.shaikh@gmail.com> wrote:
Dear All

I have query about use of Electrode with change og classification 

We have WPS for SMAW welding process for P1 material with the E 7018 electrode in that case can we use in production E7018-1 electrode 

Please help me out in interpretation

QW 404.12 (e) from a classification that requires toughness testing
to the same classification which has a suffix which indicates
that toughness testing was performed at a lower
temperature or exhibited greater toughness at the required
temperature or both, as compared to the classification
which was used during procedure qualification (i.e., a
change from E7018 to E7018‐1)

--
*With Regards
Shaikh.Hasin
Email: hasin.shaikh@gmail.com
Mobile: +91-9924562942*


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...