Re: [MW:28089] ROOT GAP QUALIFICATION WHEN QUALIFYING WPS/PQR/WPQ

Dear Sourav,

Thanks you so much for clear my doubt on this topic.

This is the only group from where i can get satisfactory answer.

Also humble request to Team, if there is any other groups related to engineering field like this,Then please share to explore  batter experience.    

On Sat, Jul 14, 2018 at 11:30 AM Souravbohray <ermechsouravbohray@gmail.com> wrote:
mr jay there is no statment regarding root gap. simple in wps u mention as per fabrication drawing in column of wps.i have experience of this nd i got guidline about this from ASME Authorised Inspector.dnt worry go ahead

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...