Re: [MW:28088] RT before and after PWFT for ASME 31.3 piping

For 1&2 not required

On Sat, 14 Jul 2018 5:12 pm krishna kamal nayan Pandey, <kkmech1987@gmail.com> wrote:
Dear Experts,

May i request you to please confirm if RT must be done before and after PWHT or only after PWHT for ASME 31.3 piping.

ASME 31.3 specify for P No. 3,4,& 5 only.I want to know for P no 1&2.




Project Spec doesn't provide this information.

Kindly assist.

Best Regards,

 

Krishana Kamal Nayan


 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...