Friday, July 13, 2018

Re: [MW:28074] This types of weld is acceptable in vessel

Dear Kanna,

As per my knowledge its acceptable but Kindly as supplier for Radiography (RA) with X-Ray Report and NDT test Certificate.

let me know if you have any quarry.

Regards and Thanks,
Hushikesh Joshi
+918460114486


On 13 July 2018 at 00:35, SRINI <kanna.qc@gmail.com> wrote:

Dear All 
Please find the attached photos below.
This type of welds is acceptable in pressure vessel.
Stiffner to nozzle weld was fallen on nozzle to flange welding.. could please advice.
 VESSEL AS PER ASME 

Regards
Kanna

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...