Re: [MW:28059] ROOT GAP QUALIFICATION WHEN QUALIFYING WPS/PQR/WPQ

Separately, There is no Root Gap qualification in code as its non-essential variable as per ASME IX.
Hence , cheers  go ahead and maintain the gap as appropriate. 

On Wed, 11 Jul 2018 at 16:16, Nithin Joseph <nithindsilva4u@gmail.com> wrote:
Dear,

There is no limit,  you can follow any root gap.

On Wed, Jul 11, 2018 at 9:04 AM, JAY <jay0000.jp@gmail.com> wrote:
Dear Team,

I have some question in my mind regarding WPS/PQR/WPQ Qualifications. Explain below.

1. I have qualified wps with(SAME SEC IX)-
    Materials : SA 240 GR 316L TO SA 240 GR 316L (P8 G1 TO P8 G1)
    Process : GTAW.(with back gauge)
    Thickness: 8 mm to 8 mm.
    Root gap: 1.6 mm
 
     Now my question is about root gap qualification,
     If i qualify WPS with above parameters having root gap 1.6.The range qualification of thickness is 4 to 16 mm. likewise is there any range for Root gap qualification?

    YOUR ASSISTANCE IN THIS MATTER WOULD BE GREATLY APPRECIATED. 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.



--
Regards,
Dsilva

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...