Sirs

-- During weld metal Analysis of ER 90 S - B9 welded on P-91 material. According to ASME SEC II part C SFA 5.28 below table. 1 , Notes-: h/i/j applicable. How to measure Nitrogen by using PMI.
Same time, is it mandatory to mention field PMI reports.
Thanks & Regards