Dear experts,
I have a prequalifed WPS for A36 material butt joint up to 32 mm thickness. Preheat mentioned there as 0deg.up to 20mm thickness and 20 to 32mm thickness is 20 deg.
But as per AWS D1.1 table 3.2, there is no preheat mentioned for base metal A36.
So what is the reference for 20 deg. Preheat for thickness 20 to 32 mm.
Please give your feedback.
Regards,
Linoy
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.
Subscribe to:
Post Comments (Atom)
[MW:35692]
Dear all Can I do MPI above painting surface for cs tank Regards, Sriram Srinivasan -- https://materials-welding.blog...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...
No comments:
Post a Comment