Friday, July 13, 2018

[MW:28071] This types of weld is acceptable in vessel


Dear All 
Please find the attached photos below.
This type of welds is acceptable in pressure vessel.
Stiffner to nozzle weld was fallen on nozzle to flange welding.. could please advice.
 VESSEL AS PER ASME 

Regards
Kanna

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS