Thursday, July 12, 2018

[MW:28064] Interpretation of EN 10217-7 ( Welded tube for pressure purpose)

Interpretation Of EN 10217-7:-

SA 312 allowed to produce welded pipe (greater than NPS 14) by forming and Welding two longitudinal sections of flat stock.While EN 10217-7 is silent for welding two longitudinal section of flat stock.
Does that mean Welded tube manufactured as per EN 10217-7 shall have a single longitudinal weld??

Thanks
Jaydeep Limbasiya
QA QC Engineer

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...