Skip to main content

Re: [MW:27864] Under Water welding

Dear Mr Muthu 
Many many thanks for your kind support. 
If you know any other brand of the electrodes please do share the information. 
Many many thanks again. 

On Sat, May 19, 2018 at 9:15 AM muthu barathi <muthu_barathi@rediffmail.com> wrote:


Dear Sir,
For under water welding you have hire divers one who have qualified in under water welding. 

Basic underwater methods

There are two basic methods for underwater welding: wet or dry, where wet welding takes place in the water and dry welding takes place in a cofferdam, drydock or habitat.

Wet underwater welding

Carried out by a diver in proper commercial weld diving equipment, wet underwater welding uses a special waterproofed welding electrode. Arc welding is used to create an arc between the electrode and the metal. The welder diver uses a tender (technician) on the surface to be in constant contact and to turn on and off current. The water provides a Faraday Cage affect to insulate the diver. The wet welding method is much less expensive than habitat welding, generally considered to be far safer and is preferred by welder divers.

Read about AquaSan Ni50, covered electrode for wet underwater welding.

Brochure

AquaSan_S-WI056-B-ENG_141023_LR (PDF document, 537 kB)

Dry underwater welding

Dry underwater welding, also known as habitat welding, is carried out in a special construction, where the water is pumped out and the chamber is pressurized. The habitat is sealed around the structure to be welded. Constructing cofferdams and habitats for dry welding is a costly business and welding operations inside them are unpopular in such confined spaces.

  • Underwater welding is a specialized field populated by highly trained welder-divers.

Risks and hazards

Both the wet and dry underwater welding methods involve risks and hazards to the welder.

  • Dry welding underwater can mean prolonged welding in a confined space requiring continuous fresh air supply
  • Wet welding involves diving in specialized welder diving equipment, which in itself is a significant risk


Thanking You.

With Warm Regards,

Muthu Barathi P.
Mobile : +918610803956 

Sent from RediffmailNG on Android




From: "Umar" <firoz.makrani@gmail.com>
Sent: Fri, 18 May 2018 19:45:41 GMT+0530
To: <materials-welding@googlegroups.com>
Subject: Re: [MW:27859] Under Water welding

No one to help?

 

 

 

With best regards,

Firoz Ahmed (Umar)

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Pieper QSI
Sent: Friday, May 11, 2018 8:35 AM
To: materials-welding@googlegroups.com
Subject: Re: [MW:27832] Under Water welding

 

I assume you will hire a diving / welding company who has experience with under water welding. Would be better to let them provide you such information instead of trying to reinvent the wheel without any knowledge!

Verstuurd vanaf mijn iPhone


Op 10 mei 2018 om 23:38 heeft Umar <firoz.makrani@gmail.com> het volgende geschreven:

Dear Experts

I want to create a WPS for Underwater welding. The material is Structural steel welding repairs by patch. The environment is marine environment.

Could someone please provide me the information like process, filler material, welding perameters etc.

Thanks in advance for your kind support.

 

 

With best regards,

Firoz Ahmed (Umar)

 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.


For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.
--
 
With Best Regards,
Umar Rashid Makrani, PMP® ,
 API653, NACE CIP-2, LEEA Registered Engineer.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Re: [MW:14950] RE: 14919] Stress relieving Rejected for 5 min less soaking time.

Dear All, I have been a CONSULTANT FOR such problem & my personal opinion is expressed as follow. I fully agree with views expressed so far. But bag to differ that " Code is a law, with engineering judgments. Hence the inspector has the rights to declare that the original HT was inadequate." Inspectors & total industry must resist the "REJECTION" . We as intellectual & having seniority must become practical. How the code will revise???. ANS.: One is experiments (Pure research) & second is such chances that gives opportunity to experiment !!! _______________________________________________________________________________________________ My understanding is that it is P1 material. In that case every pass normalizes the immediate bottom pass. Hence code requirement for P1 FOR MANDATORY SR is 32 mm & above thickness. SOLUTION:  In any case 0. After SR=PWHT no PTC testing is required as per code--Unless for low temp. vessels. That means code ...