Dear Yokesh,
I presume you were qualified a PQR for Pipe to pipe (X65 to X65) welding most likely with same electrode combination(if not, please specify). what happened to that PQR? is it pass the impact toughness? what about those impact values? if you compare these 2 scenarios(pipe to pipe and pipe to flange), you may get some conclusions. Please share if so.
Thanks in advance
Abdul Muneer
Welding Engineer
Dynamic Industries Saudi Arabia
+966550216718 (KSA)
+919895480850 (IND)
https://materials-welding.blogspot.com/