Strainer: It is wire mesh to arrest foreign material in fluid. It is normally installed at inlet of pump suction (Y type), or at inlet of static or rotating equipment. 

Filter : It is process equipment that may be a big equipment that eliminates impurities / solid material. Its filter element can be sand, cartridge, membrane. Filter has diff.l pressure indicator always. Most of the time it is spare for uninterrupted flow. Off stream to be ready for service after cleaning. 

Chandrakant Mohikar
Ex. PDO CSR. 
8446079514



On 5 Mar 2018 5:04 p.m., "Bala Murugan" <balamuruganqaqc@gmail.com> wrote:
hello ,

Filters and strainers do have a lot in common. Both products are
designed to remove suspended particles from a liquid or gas. They also
both deliver similar benefits by protecting downstream equipment and
removing impurities or contaminants that might compromise the quality
or integrity of the product.

 Both filters and strainers may be required by law or regulation for
safety or environmental reasons, used to improve the efficiency of the
system, or simply be required for practical purposes since in many
cases the flowstream would be useless without them.

Thanks,
Bala

On 3/5/18, PK M <pkmqaqc@gmail.com> wrote:
> Hello,
>
> Differance between Stainers and Fillter ?
>
> Purpose of  Stainers and Fillter ?
>
> Thanks in advance.
>
> --
> https://materials-welding.blogspot.com/
> https://www.linkedin.com/groups/122787
> ---
> You received this message because you are subscribed to the Google Groups
> "Materials & Welding" group.
> To unsubscribe from this group and stop receiving emails from it, send an
> email to materials-welding+unsubscribe@googlegroups.com.
> Visit this group at https://groups.google.com/group/materials-welding.
> For more options, visit https://groups.google.com/d/optout.
>

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...