Saturday, March 3, 2018

Re: [MW:27438] Use of Flux wire combination for SAW welding

Only difference in impact test temp. But as per ISO impact temp is 6 whereas as per ASME it is 8. Both are marked. 

On 02-Mar-2018 10:01 pm, "Perumal Govindan" <perumalgovindan@gmail.com> wrote:

Hi

F7A6-EH12K combination is not found on the picture.

The correct filler wire and flux combination for AWS classification F7A6-EH12K is "Union S EH12K - UV C 418TT.

For more information, please refer the attachment.

Regards
P Govindan

On Mar 2, 2018 15:41, "Ankur Pandey" <ankurpandey25@gmail.com> wrote:
Hi, 

Thanks for replying. Already they have mentioned AWS classification on the manufacturers marking. Please refer attached picture of manufacturer markings on flux bag.

I could not find flux wore combination as mentioned in your last mail but what I guess is that you have provided me catalogue with details of flux wire combination as I already have that.

Let me know if any other details a required.

Regards,
Ankur Pandey.

On 02-Mar-2018 12:33 PM, "Perumal Govindan" <perumalgovindan@gmail.com> wrote:

Hi

Could you please share the filler wire data sheet or batch test certificate, I believe the flux trade name (UV 18 TT) to be changed to get the AWS classification.

Further, please find the attachment for the flux wire combination.

Regards
P Govindan

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...