Re: [MW:24627] RE: 24612] Lethal service requirement


2016-04-02 22:11 GMT-06:00 pgoswami <pgoswami@quickclic.net>:

Hi Sachin,

 

I hope API RECOMMENDED PRACTICE 945, Avoiding Environmental Cracking in Amine Units is refereed in the drawings. This is an essential document for amine service .As per this document use of austenitic S.S (304L/316L) clad steel is often done for amine plant equipments, for specific set of design conditions. That's well taken care of in the details provided below.

 

As regarding fabrication, PWHT requirement is governed by the thickness of the backing material Carbon Steel, for regular amine service. From that aspect had this been a normal Amine vessel with 316L clad, exemption from PWHT would have been possible for 8 mm of C.S wall thickness.

 

Sec-VIII, UW-2 refers to mandatory PWHT for C.S/LAS vessels in "Lethal Service" . The same concept is applicable for clad vessels also, involving lethal service. Please see the latest ASME Code interpretations as below. Note there are two answers. My interpretation is to go with tracking No 9980 (since it's latest and more detailed)

 

Hope this would help.

 

Thanks.

 

 


From: sachin.sankhe@rediffmail.com [mailto:sachin.sankhe@rediffmail.com]
Sent: Friday, April 01, 2016 1:25 PM
To: materials-welding@googlegroups.com
Subject: [MW:24612] Lethal service requirement

 

Dear Friends,

 

Need your opinion on below

 

Equipment

Columns

 

Design Code

 

ASME SEC VIII Div.1

 

Process 

 

High Wet H2S service(NACE)

Wet Amine service

Very Toxic

Lethal(ASME SEC VIII, UW-2)

 

Metallurgy/Thk

Base Metal MOC=SA516 Gr.70

Thk=8mm

Clad MOC=SS316L

Clad thk=3mm

 

Problem

Is PWHT mandatory for clad vessel for above process condition?

For lethal service is PWHT not mandatory for clad vessel as per Table UCS56.1 Note (e)

 

Regards

Sachin Sankhe

 

 

 

 

 


Get your own FREE website, FREE domain & FREE mobile app with Company email.  

Know More >

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/20160401172500.21291.qmail%40f5mail-224-128.rediffmail.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/!%26!AAAAAAAAAAAYAAAAAAAAAOT5XfyRhstKvyeqQRSrfFXCgAAAEAAAAHsE2gzSxr1MjMVWF%2B9WUPABAAAAAA%3D%3D%40quickclic.net.
For more options, visit https://groups.google.com/d/optout.



--

Ing. Jose Juan Jimenez Alejandro

Cel. 8116171750

Skype: jjjimeneza

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAO5ZurKSyHWWRqWyCT7DvYN7fZZCa1q0-Sa1%2BGn_pvSuHr0fAQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

Comments

Popular posts from this blog

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

[MW:5202] RE: 5200] NDT after PWHT

------------------------------------- Interpretation:  I‑89‑14 Subject:         Section I (1986 Edition, 1987 Addenda), PW‑11,                  NDE Prior to PWHT Date Issued:     December 15, 1988 File:            BC88‑393   Question: Does PW‑11 require that NDE be performed on welds after they have been subjected to the postweld heat treatment required by PW‑39?   Reply: No, unless the conditions described in PW‑11.2.2 exist. ---------------------------------------------- Interpretation:  VIII-1-98-09 Subject:         Section VIII, Division 1 (1995 Edition, 1996 Addenda); NDE                 ...

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...