Dear All experts,

Kindly conclude....the matter because many of us have same query for GTAW.


Thanks

Ramesh Barot


Sent from my LG Mobile


------ Original message------

From: Jim Price

Date: Tue, 5 Apr 2016 08:14

To: materials-welding@googlegroups.com;

Subject:RE: [MW:24630] GTAW weld weaving


Nowhere found this is why you need to specify weave or stringer.

Weave width needs to be included.

 

Best Regards

 

Jim Price|Welding Engineer, CWI

Direct:  320.7463439| Fax: 417-862-5564

jimprice@polarcorp.com

 

 

 

 

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com]On Behalf Of Kannayeram Gnanapandithan
Sent: Saturday, April 02, 2016 2:44 AM
To: materials-welding
Subject: Re: [MW:24617] GTAW weld weaving

 

no KMJ, nowhere it is given like what u have said


THANKS & BEST REGARDS,

KG.PANDITHAN, IWE,  AWS-CWI, CSWIP 3.1,

CONSULTANT-WELDING & QUALITY

 

On Sat, Apr 2, 2016 at 12:44 PM, JIJILAL K M <jijilalkm2@gmail.com> wrote:

In general practice ,the weaving width is limited to 2.5 to 3 times the dia. of filler wire used in GTAW 


JIJILAL K.M. 

QA/QC Manager,

Thai Jurong Engineering Ltd,

KCE SPP Project,Thailand

 

 

 

On 31 March 2016 at 16:59, simon lawrence <simonlawrence08@gmail.com> wrote:

Pls confirm that Weld weaving width ,  weld weave maximum how much we can accepted in GTAW process ?

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email tomaterials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/757ab274-8b90-4e73-93a9-35e7c078e57f%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

 

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email tomaterials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHmEnHg8oBk8BuYiHw2U1%2B68_ri3QZ9EdgtUeT%2BfHN-YzEBdJg%40mail.gmail.com.


For more options, visit https://groups.google.com/d/optout.

 

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email tomaterials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eMhbo768T7d3h%2BJTE5BUwN-pNvMpHVSWcHA1i4hvcojVA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:30043] Weep hole

If weep hole is not provided in dummy pipe before welding What will happen??? -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/da251ee6-fa7f-4851-b876-cdb3834ae341%40googlegroups.com .

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .