Monday, May 18, 2015

RE: [MW:23293] PPE in orbit vlaves

The Orbit valve is a rather special "rising stem non-contacting" ball valve.

In my opinion one of the best ball valves being produced in this World.

 

It is born with only one seat, a fixed seat, and usually that seat should be upstream the flow.

Especially in services with sand and other solids in the fluid, the seat must be upstream.

Also if it used for opening where there is a large differential pressure, the valve works best with the seat upstream, because at the beginning of the opening phase, the ball is pressed away from the fixed seat rather than pressed into it.

 

I believe there are some services, where the seat should be downstream. Pls. consult the Orbit Installation, Operation and Maintenance manual, that can be found on the Internet.

 

 

 

Yours sincerely

Kristian Lund Jepsen

 

M. Sc. Mech. Eng.

Senior Chief Consultant

Piping & Mechanical

 

D +45 - 51617324

M +45 - 23402936

________________________________________

 

Ramboll

Willemoesgade 2

DK-6700 Esbjerg

Denmark

 

DK reg.no. 35128417    

 

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of hwjoshi@tce.co.in
Sent: 13. maj 2015 14:44
To: tdky167@gmail.com
Cc: materials-welding@googlegroups.com
Subject: Re: [MW:23277] PPE in orbit vlaves

 


It matters at least for globe valve for following the flow direction as marked on it..







your truly
H W JOSHI
ENGINEER MECHANICAL
TATA CONSULTING ENGINEERS LTD
MUMBAI - 400 083
TEL : 022 61148414


TDK YOKESH <tdky167@gmail.com>
Sent by: materials-welding@googlegroups.com

12-05-2015 16:07

Please respond to
materials-welding@googlegroups.com

To

"materials-welding@googlegroups.com" <materials-welding@googlegroups.com>

cc

Subject

Re: [MW:23272] PPE in orbit vlaves

 




Hello  sagar , 

So the valve has to be installed with respect to PPE not by flow direction ie. If the flow as per iso is east to west and when the valve is installed with respect to PPE the flow for valve is west to east and it doesn't matters ?? Is there a document or standard which gives detail explanation about PPE ???




On Mon, May 11, 2015 at 3:23 PM, sagar patil <sagar.tecnimont@gmail.com> wrote:
Orbit valves are single seated valves; this arrangement make the valves unidirectional.

Manufacturers of these valves mostly mark PPE on flange rims instead of flow directions.



On Thu, May 7, 2015 at 5:02 AM, TDK YOKESH <tdky167@gmail.com> wrote:
Warm Greetings folks ,

Being a welding/ material forum , I dont know whether I should be posting this .

What is PPE ( preffered Pressure End ) ??? How does it affect the flow ??? What if the flow direction and PPE  are different as per ISO?? how should the valve be installed . I mean with respect to PPE or flow direction ??? Please clarify . 

--
Best regards,
TDK YOKESH
QC INSPECTOR ( PIPING AND WELDING )
QUALITY CONTROL DEPARTMENT

Plot D1, Lumut Port Industrial Park,
Kg. Acheh, Mukim of Lumut,
Daerah Manjung, 32000 Sitiawan,
Perak Darul Ridzuan,
Malaysia
Tel No. : +601126527600
Email: tdky167@gmail.com

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to
materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to
materials-welding@googlegroups.com.
Visit this group at
http://groups.google.com/group/materials-welding.
To view this discussion on the web visit
https://groups.google.com/d/msgid/materials-welding/CAKT-TupYUac4gJpOfpFPtaE3CxW21Xn-nKesTc9QJLRN_jMTrw%40mail.gmail.com.
For more options, visit
https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAAG38UkC-i6%3DNjuyGsLm7GAG1DBs7TBAizKs8tj7ao%2BMxQ9gRQ%40mail.gmail.com.

For more options, visit https://groups.google.com/d/optout.



--
Best regards,
TDK YOKESH
QC INSPECTOR ( PIPING AND WELDING )
QUALITY CONTROL DEPARTMENT

Plot D1, Lumut Port Industrial Park,
Kg. Acheh, Mukim of Lumut,
Daerah Manjung, 32000 Sitiawan,
Perak Darul Ridzuan,
Malaysia
Tel No. : +601126527600
Email: tdky167@gmail.com

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKT-Tuo%2BScuYZ%3DKVAFfD-erwZ7Dzh8a%3DgG70vFnUwpz6fFy1rw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.


----------------------------------------------------------------------------------------------------------
Information transmitted by this E-MAIL is intended only for the use of the addressee(s) and contains information that is privileged, confidential or exempt from disclosure under applicable law. If you are not the intended recipient or it appears that this mail has been forwarded to you without proper authority, you are notified that any use or dissemination and or copying of this email in any manner is strictly prohibited and you are requested to delete this e-mail immediately.
Communicating through e-mail is not secure and capable of interception and delays. Any one communicating with TATA Consulting Engineers Ltd., and / or its subsidiaries or associates or group companies by e-mail accepts the risks involved and their consequences.
While this e-mail has been checked for all known viruses, the addressee should also scan for viruses and notify the originator of e-mail.
---------------------------------------------------------------------------------------------------------

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/OFE4BE0EA6.46FEA82B-ON65257E44.0045AC3C-65257E44.00457E25%40tce.co.in.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...