Hello  sagar , 

So the valve has to be installed with respect to PPE not by flow direction ie. If the flow as per iso is east to west and when the valve is installed with respect to PPE the flow for valve is west to east and it doesn't matters ?? Is there a document or standard which gives detail explanation about PPE ???




On Mon, May 11, 2015 at 3:23 PM, sagar patil <sagar.tecnimont@gmail.com> wrote:
Orbit valves are single seated valves; this arrangement make the valves unidirectional.

Manufacturers of these valves mostly mark PPE on flange rims instead of flow directions.



On Thu, May 7, 2015 at 5:02 AM, TDK YOKESH <tdky167@gmail.com> wrote:
Warm Greetings folks ,

Being a welding/ material forum , I dont know whether I should be posting this .

What is PPE ( preffered Pressure End ) ??? How does it affect the flow ??? What if the flow direction and PPE  are different as per ISO?? how should the valve be installed . I mean with respect to PPE or flow direction ??? Please clarify . 

--

Best regards,

TDK YOKESH

QC INSPECTOR ( PIPING AND WELDING )

QUALITY CONTROL DEPARTMENT

https://encrypted-tbn0.gstatic.com/images?q=tbn:ANd9GcQ7lSlmn1ExpyOpkX2RaZW-T5JttIFRfJMtPb23EzPZOQxDBU2w8PO-rDQ

Plot D1, Lumut Port Industrial Park,

Kg. Acheh, Mukim of Lumut,

Daerah Manjung, 32000 Sitiawan,

Perak Darul Ridzuan,

Malaysia

Tel No. : +601126527600

Email: tdky167@gmail.com

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKT-TupYUac4gJpOfpFPtaE3CxW21Xn-nKesTc9QJLRN_jMTrw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAAG38UkC-i6%3DNjuyGsLm7GAG1DBs7TBAizKs8tj7ao%2BMxQ9gRQ%40mail.gmail.com.

For more options, visit https://groups.google.com/d/optout.



--

Best regards,

TDK YOKESH

QC INSPECTOR ( PIPING AND WELDING )

QUALITY CONTROL DEPARTMENT

https://encrypted-tbn0.gstatic.com/images?q=tbn:ANd9GcQ7lSlmn1ExpyOpkX2RaZW-T5JttIFRfJMtPb23EzPZOQxDBU2w8PO-rDQ

Plot D1, Lumut Port Industrial Park,

Kg. Acheh, Mukim of Lumut,

Daerah Manjung, 32000 Sitiawan,

Perak Darul Ridzuan,

Malaysia

Tel No. : +601126527600

Email: tdky167@gmail.com

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKT-Tuo%2BScuYZ%3DKVAFfD-erwZ7Dzh8a%3DgG70vFnUwpz6fFy1rw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...