To the best of my knowledge NBIC has not such a provision for P91

Sent from my BlackBerry 10 smartphone.
From: pgoswami
Sent: Σάββατο, 9 Μαΐου 2015 - 16:43
To: materials-welding@googlegroups.com
Reply To: materials-welding@googlegroups.com
Subject: [MW:23245] RE: 23237] Welding P91 without PWHT

Hi Jose,
 
Strictly as per all design and construction codes as well as the  various recommended practices, "PWHT" on grade 91 steel is must after welding.
 
Off late there had been thoughts to push " Temper bead repair technique in NBIC " by EPRI (Electric Power Research Institute).You may search in google under" temper bead welding on grade-91 steel or other suitable titles" to get more details.
 
In order to achieve those one has to have "PQR " qualified separately as well as the welding  consumables may be different.Which may need some lead time and preparations.
 
I would think the trouble free option without any prior preparations would be to PWHT the welds.
 
Please see the link below, whether I' ad posted the link to NBIC document containing an EPRI presentation.
 
Thanks,
 
 
Pradip Goswami, P.Eng,IWE
Welding & Metallurgical Engineer/Specialist
Ontario, Canada
 
 
https://www.linkedin.com/grp/post/122787-198284274

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of José Luís Ferreira
Sent: Friday, May 08, 2015 10:15 AM
To: materials-welding@googlegroups.com
Subject: [MW:23237] Welding P91 without PWHT

Is there an alternative to weld P91 to P91 (Cr-Mo-V) without performing PWHT? I need to weld (repair) small valves (socket welds) in field.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/70192939-7f6a-40f3-be22-dec8ccbc00ad%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/737FEF0E4ED14707AC48088754970CE4%40homepg.
For more options, visit https://groups.google.com/d/optout.

This message contains confidential information. To know more, please click on the following link: http://disclaimer.bureauveritas.com

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...