Dear

WPS is restricted to what for it is written, some of the WPS written for fillet, Groove,  fillet + Groove 

These are based on Limitation by Qualified PQR 

For your query

what is the reference code for PQR qualification , with that code if the PQR limitations allow to use for both just rewriting the WPS  as per your requirement with PQR limitation will serve you


Regards
M.Sathiyanarayanan





 

On Sat, May 23, 2015 at 7:42 AM, meisam shokri arfaei <meisamshokri@gmail.com> wrote:
I Think that the question was about welding and not about qualification.

Whenever a WPS (whether Standard, pre-qualified or qualified) prepared, the manufacturer allow to use it only with values or in the range which mentioned in that WPS.

The qualification has a different story. One or more WPS's may qualified with single PQR (or number of PQR's which are less than the number of WPS's and in some cases one PQR for each WPS) under the criteria and qualification rules of the design and/or qualification code. 

So, in summary, if you have a WPS for welding a groove weld, you allowed to use it just for that. For a fillet weld you should prepare a new WPS. however both may qualified with a single WPS.


Regards



On Fri, May 22, 2015 at 9:41 AM, anosh wankhade <anosh_wankhade@rediffmail.com> wrote:

Agreed with Dr. Georgious,

This is listed as non essential Variable in ASME section IX.
Please refer QW : 4.2.30 

Regards,

Anosh Wankhade

From: george.dilintas@gr.bureauveritas.com
Sent: Thu, 21 May 2015 16:54:53
To: materials-welding@googlegroups.com
Subject: Re: [MW:23005] WPS with groove welding will also qualify Fillet welding.

When ASME is the Code, yes
This is not the case for EN 15614-1

best regards

Dr. Georgios Dilintas

Authorized Nuclear Inspector
Authorized Inspector Supervisor

I&F REGIONAL TECHNICAL MANAGER
BUREAU VERITAS PIRAEUS - GREECE

Tel: +30 210 40 63 113 /4 /5
Fax: +30 210 40 63 118
Cell: +30 69 44 64 62 04


Inactive hide details for Mohammed Ghani ---21/05/2015 13:13:43---Dear Experts, Can any one suggest if Groove welding WPS will Mohammed Ghani ---21/05/2015 13:13:43---Dear Experts, Can any one suggest if Groove welding WPS will also allow welding with

From: Mohammed Ghani <ghani386@gmail.com>
To: materials-welding@googlegroups.com
Date: 21/05/2015 13:13
Subject: [MW:23002] WPS with groove welding will also qualify Fillet welding.
Sent by: materials-welding@googlegroups.com





Dear Experts, 

Can any one suggest if Groove welding WPS will also allow welding with fillet. please guide with reference standard clause.

--
Thanks and Regards, ?

Mohammed Ghani,


CSWIP 3.1 / BGAS L-2 / ISO 9001:2008 QMS LA.

Mechanical Inspector,
BUREAU VERITAS.


ü
 Please consider the environment before printing this email.
 "Be the change you wish to see in the world"
---Mahatma Gandhi---

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to
materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to
materials-welding@googlegroups.com.
Visit this group at
http://groups.google.com/group/materials-welding.
To view this discussion on the web visit
https://groups.google.com/d/msgid/materials-welding/CAG7AWVjjPwZ%2BkvBBQ-mQ1p1XV0tjtSv4jh8vqu-icwtVMpD%2B7g%40mail.gmail.com.
For more options, visit
https://groups.google.com/d/optout.

This message contains confidential information. To know more, please click on the following link: http://disclaimer.bureauveritas.com

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/OFE44D54DE.B3B1B3E4-ONC2257E4C.003EA35C-C2257E4C.003EB065%40LocalDomain.
For more options, visit https://groups.google.com/d/optout.

Get your own FREE website, FREE domain & FREE mobile app with Company email.  
Know More >

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1432207493.S.24917.13610.f4-235-222.1432271486.12684%40webmail.rediffmail.com.

For more options, visit https://groups.google.com/d/optout.



--
M. Shokri Arfaei
ISA-ISTS - Metallurgy Lab. Manager
ASNT NDT Level III
International Welding Engineer

Tel.: +98 21 66282127
Fax: +98 21 66282779
Mob.:+98 912 1394023




--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAC8uMtsZ1%3DvgR1C50V2LFRBs8f%2Bwmn8vW-pSRZH2XDZdEzD6VQ%40mail.gmail.com.

For more options, visit https://groups.google.com/d/optout.



--
Thanks and Regards
M.Sathyanarayanan

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzo-kt%2BWi20LD0fbO1-v_eDpCT%2B491u2dq5Txwh2B%2BDCq2Yfw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...