Monday, May 25, 2015

Re: [MW:23028] requalified wps aws d1.1

my WPS is according to AWS D1.1 . for structural steel construction .

So, if I do not need to test again PQR , I just rewrite welding process layer .

Thanks all experts

Vào 23:35:43 UTC+7 Thứ Bảy, ngày 23 tháng 5 năm 2015, kannayeram gnanapandithan đã viết:

As long as if u are not exceed deposited weldmetal thickness for each process u need not qualify

On 23-May-2015 2:30 pm, "anosh wankhade" <anosh_w...@rediffmail.com> wrote:
Dear Jerry,

In case the WPS is qualified according to ASME section IX, no need to re qualify WPS.

Just make necessary changes in WPS and use to same PQR.

Regards,

Anosh   

From: JERRY TUAN <jerr...@gmail.com>
Sent: Sat, 23 May 2015 10:24:11
To: material...@googlegroups.com
Subject: [MW:23014] requalified wps aws d1.1
Dear experts,
 i have one question, and I need your help. Thanks first
My WPS is SAW, qualified for tube OD = 2000mm spiral welding pipe sheet pipe.

my WPS is for splicing 2 pipe ( that mean you connecting 2 pipe together )
 the joint design is X bevel
and the layer step of welding is: 
1. GMAW at root
2. cover out side SAW
3. cover inside SAW

so now if I want to change the step welding layer to:
1. GMAW at root
2. cover inside SAW
3.cover out side SAW
 and all other parameters are not change

=>> so my question is . Do I need to requalify my WPS, OR I just rewrite WPS and keep the original PQR,no need to test PQR again


THANKS FOR YOUR HELP.
Jerry.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/2bba4822-fb64-438b-b888-6eae83f0ca2f%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

Get your own FREE website, FREE domain & FREE mobile app with Company email.  
Know More >

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1432356851.S.12360.3891.f4-235-146.1432371551.17566%40webmail.rediffmail.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/6f292b37-5087-4979-8cb6-edccaa077eac%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...