im sorry ASME SEC IX QW254&255.




On Saturday, May 23, 2015 12:48 PM, 'HAMID HAMIDI' via Materials & Welding <materials-welding@googlegroups.com> wrote:


asme sec iiiv qw254 & 255 .no need to retest no problem.



On Saturday, May 23, 2015 10:59 AM, Ken Waterhouse <waterhouse.ken@gmail.com> wrote:


Hi Jerry, 

Can you clarify to which code or standard the WPS is written? 

Regards
KW

On Saturday, May 23, 2015 at 5:54:14 AM UTC+1, JERRY TUAN wrote:
Dear experts,
 i have one question, and I need your help. Thanks first
My WPS is SAW, qualified for tube OD = 2000mm spiral welding pipe sheet pipe.

my WPS is for splicing 2 pipe ( that mean you connecting 2 pipe together )
 the joint design is X bevel
and the layer step of welding is: 
1. GMAW at root
2. cover out side SAW
3. cover inside SAW

so now if I want to change the step welding layer to:
1. GMAW at root
2. cover inside SAW
3.cover out side SAW
 and all other parameters are not change

=>> so my question is . Do I need to requalify my WPS, OR I just rewrite WPS and keep the original PQR,no need to test PQR again


THANKS FOR YOUR HELP.
Jerry.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/222838b6-bef2-4804-a479-803b7c18cb2f%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.


--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/419506569.855225.1432368303762.JavaMail.yahoo%40mail.yahoo.com.
For more options, visit https://groups.google.com/d/optout.


No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...