Re: [MW:23011] We can use AWS D 1.1 pre-qualified WPS for SA 387 Gr 12 plate material ?

Dear Experts,

We can use AWS D 1.1 pre-qualified WPS for SS400 ( or JIS SKK400) cause i do not know what  group it is, plate material ?

Thanks,
 
Jerry.

Vào 17:25:11 UTC+7 Thứ Hai, ngày 18 tháng 5 năm 2015, Anosh Wankhade đã viết:



Dear Yem,

Better to use ASME for it as this material is not listed in AWS D 1.1

Regards,

Anosh

From: PK M <pkm...@gmail.com>
Sent: Sun, 17 May 2015 15:23:18
To: material...@googlegroups.com
Subject: [MW:23291] We can use AWS D 1.1 pre-qualified WPS for SA 387 Gr 12 plate material ?
Dear Experts,

We can use AWS D 1.1 pre-qualified WPS for SA 387 Gr 12 plate material ?

Thanks,
 
Yem.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFoQ_ncP1%3DjeXU54sdtNCRRswjmUKXN1BDHJ%3D%3DXP8P6vwZjt9A%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

Get your own FREE website, FREE domain & FREE mobile app with Company email.  
Know More >

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1e4e09ac-5ae6-4bd4-a693-535efa5357bb%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...