Monday, May 18, 2015

[MW:23297] Welding & pwht time difference in P-91 Material

Dear All,
Can anybody inform code reference in B-31.1 welding & pwht time diference. Client is asking for 14 days.
Is it mandatory in code

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAB%3DAs8%3D5YTF7j9_HXs5PJzN2GMNjA8qZrrEAti7aO8ca4bCWTg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...