[MW:23292] Weld overlay of Duplex Stainless steel over 316L:

A vessel we have, had the issue of preferential weld erosion corrosion as compared to parent metal (shell course/dished head), up to the height of ~3.5m from bottom dished head. It was repaired by welding. Require advice on suitability of weld overlaying of above specified affected area (say 3.5 to 4m height) by duplex /super duplex stainless steel (e.g. 2707 grade).

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/d4280196-1950-4afc-aeea-0c64ce2f765c%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...